Vinylpyridine MechanicalProperty Lateral LightEmission OpticalModulator temp Lateral_Force_Microscopy molecule amplitude_modulation self_healing CNT Techcomp rubber Conduct margarine conductive Cobalt-dopedIronOxide InsulatorFilm Wafer SSRM Spincast Indium_tin_oxide dielectric_trench Etch Hair Terrace H-BN ElectrostaticForceMicroscopy Pyroelectric Indent TCS PpLdpe GlassTemperature Graphite Neodymium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polycrystalline ferroelectric BCZT
Scanning Conditions
- System: NX12
- Scan Mode: PFM
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.4Hz
- Pixel: 256×256
- Sample bias sweep range for Piezoresponse curve: -10V ~ +10V